Hi Bob, the disk plate is tungsten, I’ll update the linked slide with a more comprehensive set of electrode material combinations and highlight if the witness plate was wetted or not. The SS electrode is significantly more energetic. I tried capturing the TDM response on a W anode that fit into a 2-level Bagel, only captured the pre-BL signal which is just as interesting in my opinion. Will add to the slides as well.

Expand full comment

Thanks, that is great. I think I will make a page for this work.

Expand full comment

Slides look good. Will properly review tomorrow

Expand full comment

Caught the maker-breaker pretzel on TDM scope! - spoiler alert: it's a chaotic signal. Slides up to date.

Expand full comment

Awesome.

Where are you based? I'd like to take a look (SEM/EDX) at some of those targets.

Expand full comment

In Australia. I'll start wearing some gloves when I'm handling the next few so I don't get my grubby fingers all over them. Just let me know where to post them, I think you have my email?

Expand full comment

Should do.

If you can get them to California by the 28th, I can take a look at them.

Expand full comment

Will have it in the mail in the morning. I wanted to include the a bismuth bead sample, so I reproduced my earlier Adamenko-style experiment and it appears that I disappeared some bismuth??!! I also exploded one so have included that in the samples, marked Bi Bead. Vid link in the ppt.

Expand full comment

Cool, thanks. Do you have a sample of the before material on the Bi?

Expand full comment

Will include it!